BS EN 4825. Aerospace series. Steel X12CrNiMoV12-3 (1.4933). Air melted and consumable electrode remelted. Hardened and tempered. Bar. De = 150 mm. 900 MPa = Rm = 1100 MPa

Summary

Corrosion tests;Compression set;Mixing;Tear tests;Elastic constants;Elongation;Tensile strength;Density;Hardness testing;Approval testing;Qualification approval;Quality assurance;Quality assurance systems;Synthetic rubber;Natural rubber;Air transport engineering;Dimensions;Defects;Ships;Water transport engineering;Steels;Factor of safety;Mass;Loading;Designations;Ladders;Installation;Maritime structures;Water transport engineering components;Climbing devices;Aerospace transport;Test methods;Cables (electric);Aircraft components;Measurement;Contrast (optical);Air;Melting;Electrodes;Testing methods;Testing;Environmental testing;Durability;Sleeving (electrical);Diameter;Shape;Alloys;Non-ferrous alloys;Nickel alloys;Circuit-breakers;Temperature;Electrical measurement;Cable ties;Launching facilities (aerospace);Surfaces;Treatment;Surface treatment

Technical characteristics

Publisher British Standards Institution (BSI)
Publication Date 04/05/2012
Page Count 9
Themes Surface treatment
EAN ---
ISBN ---
Weight (in grams) ---