ASTM A770/A770M-03(2007)
Summary
1.2 The values stated in either inch-pound units or SI units are to be regarded as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of the other. Combining values from the two systems may result in nonconformance with the specification.
1.3 This specification is expressed in both inch-pound and SI units. However, unless the order specifies the applicable “M” specification designation (SI units), the material shall be furnished to inch-pound units.
Rationale:
This specification covers procedures and acceptance standards for the determination of reduction of area using steel plates as tension test specimen. The tension testing method shall provide a measure of the resistance of a steel plate to lamellar tearing. Alternative test specimen may be used in place of the standard test specimen. Several types of test specimen shall have specified values of plate thickness, diameter, minimum radius, and length of reduced section.
Technical characteristics
| Publisher | American Society for Testing and Materials (ASTM International) |
| Publication Date | 05/10/2003 |
| Confirmation Date | 11/01/2007 |
| Collection | |
| Page Count | 5 |
| EAN | --- |
| ISBN | --- |
| Weight (in grams) | --- |