Standard Specification for Pressure-Vessel Plates, Quenched-and-Tempered, Manganese-Chromium-Molybdenum-Silicon Zirconium Alloy Steel
Summary
1.1 This specification covers high-strength quenched and tempered alloy steel plates intended for use in fusion welded pressure vessels.
1.2 Plates under this specification are available in three classes having different strength levels as follows:
| Yield | Tensile | |
| Strength, | Strength, | |
| min, | min, | |
| Class | ksi [MPa] | ksi [MPa] |
| 1 | 80 [550] | 97 [670] |
| 2 | 90 [620] | 107 [740] |
| 3 | 100 [690] | 115 [795] |
1.3 The thickness of plates under this specification is limited to a maximum of 2 in. [50 mm].
1.4 The values stated in either inch-pound units or SI units are to be regarded separately as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of the other. Combining values from the two systems may result in nonconformance with the specification.
Technical characteristics
| Publisher | American Society for Testing and Materials (ASTM International) |
| Publication Date | 01/01/1990 |
| Confirmation Date | 01/01/2001 |
| Collection | |
| Page Count | 3 |
| EAN | --- |
| ISBN | --- |
| Weight (in grams) | --- |
No products.
Previous versions
01/01/1990
Superseded
, Reaffirmed
Historical
01/01/1990
Superseded
, Reaffirmed
Historical