Active
Standard
Most Recent
BS L 102:1971
Specification for bars and extruded sections of aluminium-copper-magnesium-silicon-manganese alloy (solution treated and aged at room temperature) (not exceeding 200 mm diameter or minor sectional dimension) (Cu 4.4, Mg 0.5, Si 0.7, Mn 0.8)
Summary
Manganese-containing alloys;Metal sections;Solution heat treatment;Bars (materials);Silicon-containing alloys;Dimensions;Hardness;Magnesium-containing alloys;Air transport engineering;Aluminium alloys;Chemical composition;Mechanical properties of materials;Heat treatment;Copper-containing alloys
Technical characteristics
| Publisher | British Standards Institution (BSI) |
| Publication Date | 08/31/1971 |
| Page Count | 8 |
| Themes | Copper-containing alloys |
| EAN | --- |