Superseded
Standard
Historical
DIN EN 1939:2003-12
Self adhesive tapes - Determination of peel adhesion properties; German version EN 1939:2003
Summary
The document specifies a series of methods for the determination of peel adhesion properties of self adhesives tapes. Annexes A and B specify further variations in the testing protocol according to specific conditions. This European Standard contains: Method 1: Self adhesive tapes - Measurement of peel adhesion from stainless steel at an angle of 180°; Method 2: Self adhesive tapes - Measurement of peel adhesion from its own backing at an angle of 180°; Method 3: Self adhesive tapes - Measurement of peel adhesion of double sided and transfer tapes at an angle of 180°; Method 4: Self adhesive tapes - Measurement of adhesion of the liner to an adhesive tape at an angle of 180°. Together with Annex A: Self adhesive tapes - Measurement of peel adhesion from a surface at low temperature; Annex B: Self adhesive tapes - Measurement of peel adhesion from a surface at an angle of 90°. A guide to the use of these methods and annexes is given in Table 1.
Technical characteristics
| Publisher | Deutsche Institut für Normung e.V. (DIN) |
| Publication Date | 12/01/2003 |
| Cancellation Date | 09/01/2019 |
| Page Count | 18 |
| EAN | --- |
| ISBN | --- |
| Weight (in grams) | --- |
No products.
Previous versions
01/12/2003
Superseded
Historical
01/07/2002
Superseded
Historical