Superseded
Standard
Historical
NBN EN 683-2:2007
Aluminium and aluminium alloys - Finstock - Part 2: Mechanical properties
Summary
This document specifies the mechanical properties of wrought aluminium and wrought aluminium alloy finstock.
The chemical composition limits of these materials are specified in EN 573-3, unless otherwise agreed between supplier and purchaser.
The designations of wrought aluminium and wrought aluminium alloys and the temper designations used in this standard are specified in EN 573-3, and the temper designations are defined in EN 515.
The chemical composition limits of these materials are specified in EN 573-3, unless otherwise agreed between supplier and purchaser.
The designations of wrought aluminium and wrought aluminium alloys and the temper designations used in this standard are specified in EN 573-3, and the temper designations are defined in EN 515.
Technical characteristics
| Publisher | Bureau de Normalisation Belge (NBN) |
| Publication Date | 01/31/2007 |
| Cancellation Date | 06/30/2007 |
| Page Count | 15 |
| EAN | --- |
| ISBN | --- |
| Weight (in grams) | --- |