Active
Standard
Most Recent
NBN EN ISO 2566-2:2021
Steel - Conversion of elongation values - Part 2: Austenitic steels (ISO 2566-2:2021, Corrected version 2022-05)
Summary
This document specifies a method of converting room temperature percentage elongations after fracture obtained on various proportional and non-proportional gauge lengths to other gauge lengths.
Formula (1), on which conversions are based, is considered to be reliable when applied to austenitic stainless steels within the tensile strength range 450 to 750 N/mm2 and in the solution treated condition.
These conversions are not applicable to:
a) cold reduced steels;
b) quenched and tempered steels;
c) non-austenitic steels.
These conversions are not applicable when the gauge length exceeds 25vS0 or where the width to thickness ratio of the test piece exceeds 20.
Formula (1), on which conversions are based, is considered to be reliable when applied to austenitic stainless steels within the tensile strength range 450 to 750 N/mm2 and in the solution treated condition.
These conversions are not applicable to:
a) cold reduced steels;
b) quenched and tempered steels;
c) non-austenitic steels.
These conversions are not applicable when the gauge length exceeds 25vS0 or where the width to thickness ratio of the test piece exceeds 20.
Technical characteristics
| Publisher | Bureau de Normalisation Belge (NBN) |
| Publication Date | 12/25/2021 |
| Cancellation Date | 06/30/2022 |
| Page Count | 45 |
| EAN | --- |
| ISBN | --- |
| Weight (in grams) | --- |
Replaces
29/09/1999
Superseded
Historical
Previous versions
29/09/1999
Superseded
Historical