Superseded
, Reaffirmed
Standard
Historical
SAE AMS 2759/2F:2014-04-23
Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher
Summary
This specification, in conjunction with the general requirements for steel heat treatment covered in AMS2759, establishes the requirements for heat treatment of low-alloy steel parts to minimum ultimate tensile strengths of 220 ksi (1517 MPa) and higher. Parts are defined in AMS2759.
Notes
Approuvée 2014-04-23.
Technical characteristics
| Publisher | SAE International |
| Publication Date | 05/17/2010 |
| Confirmation Date | 04/23/2014 |
| Cancellation Date | 04/23/2014 |
| Page Count | 13 |
| Themes | Aerospace |
| EAN | --- |
| ISBN | --- |
| Weight (in grams) | --- |