Superseded
Standard
Historical
SAE AMS 5704K:2015-01-14
Nickel Alloy, Corrosion and Heat-Resistant, Forgings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated
Summary
This specification covers a corrosion and heat-resistant nickel alloy in the form of forgings 3.25 inches (82.6 mm) and under, and forging stock of any size. (See 8.5).
Technical characteristics
| Publisher | SAE International |