DIN EN 13108-5:2006-08
Bituminous mixtures - Material specifications - Part 5: Stone Mastic Asphalt; German version EN 13108-5:2006.
Summary
This Standard specifies requirements for mixtures of the mix group stone mastic asphalt. It deals also with the selection of the constituent materials. Stone mastic asphalt comprises gap-graded asphalt mixtures with bitumen as a binder, which are composed of a coarse crushed aggregate skeleton bound with a mastic mortar. Stone mastic asphalt is not pourable. After laying stone mastic asphalt mixture has to be compacted. The ratio of crushed to natural fine aggregate is normally >= 1:1. Stone mastic asphalt can be used for most kinds of traffic and in most kinds of climates on roads, airfields and other trafficked areas.
Notes
Applies in conjunction with DIN EN 13108-20 (2006-07), DIN EN 13108-21 (2006-07)
Technical characteristics
| Publisher | Deutsche Institut für Normung e.V. (DIN) |
| Publication Date | 08/01/2006 |
| Cancellation Date | 12/01/2016 |
| Page Count | 32 |