Superseded
, Reaffirmed
Standard
Historical
SAE AMS 5709H:2013-12-02
Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution, Stabilization, and Precipitation Heat Treated
Summary
This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, forgings, and forging stock.
Technical characteristics
| Publisher | SAE International |
| Publication Date | 12/02/2013 |
| Confirmation Date | 12/02/2013 |
| Page Count | 6 |
| Themes | Aerospace |
| EAN | --- |
| ISBN | --- |
| Weight (in grams) | --- |