Superseded
Standard
Historical
SAE AMS 5709J:2019-09-04
Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution, Stabilization, and Precipitation Heat Treated
Summary
This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, forgings, and forging stock.
Technical characteristics
| Publisher | SAE International |
| Publication Date | 09/04/2019 |
| Cancellation Date | 09/04/2019 |
| Page Count | 6 |
| EAN | --- |
| ISBN | --- |
| Weight (in grams) | --- |
Replaces
02/12/2013
Superseded
, Reaffirmed
Historical
Previous versions
04/09/2019
Superseded
Historical
02/12/2013
Superseded
, Reaffirmed
Historical