SAE AMS 5709K:2025-05-03
Nickel Alloy, Corrosion- and Heat-Resistant, Bars and Forgings, 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B, Consumable Electrode or Vacuum Induction Melted, 1975 °F (1079 °C) Solution Heat Treated, Stabilized, and Precipitation Heat Treated
Summary
This specification covers a corrosion- and heat-resistant nickel alloy in the form of bars and forgings in the solutioned, stabilized, and precipitation heat-treated condition. Stock for forging shall be in the condition ordered.
Technical characteristics
| Publisher | SAE International |
| Publication Date | 05/03/2025 |
| Page Count | 7 |
| EAN | --- |
| ISBN | --- |
| Weight (in grams) | --- |